On 05/07/2014 05:06 PM, Patrik D'haeseleer wrote:
> On Monday, May 5, 2014 5:02:44 PM UTC-7, Avery wrote:
>
> conductivity, unless it is really really low, is not going to be an issue compared to the resistance of the gel/buffer.
>
> 316 stainless wire works pretty well. it is a stainless steel.
>
>
> Ditto on using stainless steel.
Has anyone tried Monel alloys?
They are >63% nickel and copper and other for the remainder.
They ignore sea water weather corrosion, so maybe are good for electrodes. One use has
been on aircraft for keeper wire that stops nuts coming off from vibration, so it is
available as wire as a standard sort of low cost product. Stainless steels are
mostly >75% iron, so they are lower cost, but -- when comparing to platinum...not much
difference.
--
-- You received this message because you are subscribed to the Google Groups DIYbio group. To post to this group, send email to diybio@googlegroups.com. To unsubscribe from this group, send email to diybio+unsubscribe@googlegroups.com. For more options, visit this group at https://groups.google.com/d/forum/diybio?hl=en
Learn more at www.diybio.org
---
You received this message because you are subscribed to the Google Groups "DIYbio" group.
To unsubscribe from this group and stop receiving emails from it, send an email to diybio+unsubscribe@googlegroups.com.
To post to this group, send email to diybio@googlegroups.com.
Visit this group at http://groups.google.com/group/diybio.
To view this discussion on the web visit https://groups.google.com/d/msgid/diybio/536AEFD3.4000304%40industromatic.com.
For more options, visit https://groups.google.com/d/optout.
Re: [DIYbio] Re: Non-Platinum Electrophoresis Electrodes That Don't Degrade
7:45 PM |
Subscribe to:
Post Comments (Atom)






0 comments:
Post a Comment